TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 10 May 2005 07:51:30 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, David Fish <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
David Fish <[log in to unmask]>
Parts/Attachments:
text/plain (88 lines)
Steve



Heavy-duty nickel /nickel steel are commonly welded to batteries as terminal
strips for better conductivity and corrosion resistance.  We quadruple
spot-weld each cell terminal with a dual-pulse spot welder.



We have never welded to AA batteries.  [AA have a fairly short life and are
not rechargeable, bla, bla, bla.  If we did, we'd probably just use solder.
Although, we think AA have a solid cathode, polycarbonmonofluoride or
manganese dioxide, like a solid cathode lithium battery.  So they should
take weld.] We have welded to:

* Solid cathode lithium batteries [but not liquid cathode]

* Li-ion, Li-Polymer, Ni-MH, and NiCd



Dave Fish





----- Original Message -----
From: "Stephen Gregory" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, May 06, 2005 11:50 AM
Subject: [TN] Weldable solder terminals


> Hi All!
>
> One of our project engineers emailed me with a question;
>
> "Steve, You know a lot of people in the industry.  Do you think one of
them
> would know what material to use to make weldable solder terminals?
> They would be tack welded to AA batteries and then have a wire soldered to
> it."
>
> Can anyone help?
>
> Kind regards,
>
> -Steve Gregory-
> Senior Process Engineer
> LaBarge Incorporated
> Tulsa, Oklahoma
> (918) 459-2285
> (918) 459-2350 FAX
> __________________________________________________________________
> This message may contain information that is privileged and confidential
to
> LaBarge, Inc.  It is for use only by the individual or entity named above.
> If you are not the intended recipient, you may not copy, use or deliver
> this message to anyone.  In such event, you should destroy the message and
> kindly notify the sender by reply e-mail.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2