Rich, look in IPC-HDBK-001, the companion to J-STD-001. Section 4 is on
fluxes and has a listing of the common dicarboxylic acids used in fluxes.
That table was based on articles published by Al Schneider at Alpha Metals.
Doug Pauls
Richard
Kraszewski
<[log in to unmask] To
COM> [log in to unmask]
Sent by: TechNet cc
<[log in to unmask]>
Subject
[TN] IPC table of Organics acids
05/06/2005 12:14
PM
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Richard
Kraszewski
<[log in to unmask]
COM>
While I have and can locate several tables of organic acids commonly
used in soldering fluxes & pastes, etc., I seem to recall that some IPC
document contained a rather substantial table of these acids and some of
their physical properties.
Does this sound familiar to anyone?
Which one?
Rich K / KEDS
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------