Hi Bob,
First, with ENIG you do not solder to gold, but to the underlying nickel;
Second, soldering to Ni requires more thermal energy, thus higher temperatures, and that is really bad news on top of the T-increase necessary for LF-solders;
Third, the 'black pad' issue will not go away with LF-solderas,but actually may become worse.
Thus, Immersion Ag is a good choice.
Werner Engelmaier
-----Original Message-----
From: Jeffrey Bush <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, 27 Apr 2005 07:14:42 -0400
Subject: Re: [TN] gold vs copper plating on pcb's
If you stick with ENIG and do not test Immersion Silver then I am sure
you will be doing future testing to combat the issues with ENIG. Monies
are being put into the development if silver and several toughed
formulas are coming out that have excellent resistance to TC and do not
have the issues associated with ENIG. OSP is also seeing some
development, but I do not see this as a viable alternative today.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice: 802.257.4571.21 Fax: 802.257.0011
http://www.vtcircuits.com
-----Original Message-----
From: Bob Arciolla [mailto:[log in to unmask]]
Sent: Tuesday, April 26, 2005 4:41 PM
To: [log in to unmask]
Subject: [TN] gold vs copper plating on pcb's
Good Afternoon all,
Our company will be switching over to lead free and we have received
sample pcb's from one of our vendors and one board has gold (ENIG) for
the traces and one has copper (OSP). From some of the emails I have seen
on Technet it appears that gold is what most of companies are going to
be using? Is this correct or is there some other materials we should be
looking into to use? Is the gold more reliable than the copper?
Any input would be greatly appreciated.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
Regards, Bob
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|