If you're in the U.K. try Invisitech at http://www.invisitech.co.uk
I used to use them for this kind of thing on gold edge connectors.
Regards,
===== Original Message from [log in to unmask] (TechNet E-Mail Forum) at
20/04/05 18:24
>Hi T'Netters;
>One of our divisions experienced a "taping error" when masking gold plated
>contacts prior to wave solder.
>They now have solder coated, gold plated contacts.
>
>I know there used to be some outfits out there that could rework/repair
>this type of problem.
>Does anyone have any contacts, recommendations, (horror stories), etc. that
>might be able to correct this problem?
>TIA,
>Regards,
>Rob
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet
Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
>-----------------------------------------------------
-----------------------------------------------------------------------
Peter Barton
Senior Process Engineer
ACW Technology Ltd
Dinas Isaf West
Tonypandy
Mid Glamorgan. CF40 1XX Wales
Tel: 01443 425275 (direct)
Fax: 023 8048 4882
International Tel : +44 1443 425200
International Fax : +44 23 8048 4882
Website/URL: www.acw.co.uk
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|