That's an interesting one. Sounds like something is used to promote the
copper adhesion to Teflon. Probably dissolved away during etching and
also attacked by the alkaline Vigon. Do you know the copper treatment?
If it's yellow, it might be zinc, which could conceivably be attacked by
a strong alkali, being amphoteric. Brown-blue--reddish sounds like
copper oxide. I suggest an urgent e-mail to Dr Wack and to the laminate
maker.
Brian
Ingemar Hernefjord (KC/EMW) wrote:
> Hi all,
> anyone who have this experience?
> A. Peel fresh PWB: high force needed, white stuff left on board. Soft like butter. Copper underside yellowish.
> B. Peel used PWB: much lower force needed, no white stuff left on board. Copper underside brown-blue-redish.
>
> Reason for asking is this. We suspect that something bleeds out from beneath the copper traces during the
> VIGON cleaning. Not much, but sometimes creating kind of 'grease' along the copper traces. Therefore, I'm
> interested in the interface between the copper and the teflon. What stuff can there be that changes from white to colourless, and may be dissolved by VIGON.
>
> Sending two pics to the always and amazingly tolerant, patient and positive S.G.
>
> Ingemar Hernefjord
> Ericsson Microwave Systems
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|