I can't comment on the risk of igniting the vapors when you strike an
arc, but I have watched welders weld empty gasoline tanks, and natural
gas pipelines. One method filled the tank full of water before welding
the leak shut. (Welding can be done underwater as well) Another method
was to pull the service truck up to the ditch, hook a hose up to the
exhaust of the truck and run it into the ditch for an unspecified amount
of time before attempting the weld. I won't vouch for their
intelligence, but professional welders I've run into are sure good at
what they do. And if your tank is anything other than mild steel, I
wouldn't attempt the weld myself, rather use a professional instead.
Ryan Grant
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Gregory
Sent: Tuesday, April 19, 2005 11:49 AM
To: [log in to unmask]
Subject: [TN] Welding and Vapor Phase fluid
Hello all,
I need to grind and re-weld a bracket in my vapor phase machine and was
wondering what precautions to take? There is a very thin residual amount
of
VP fluid at the bottom of the tank after draining.
Any takers?
Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)212-0844 cell
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|