TECHNET Archives

April 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 29 Apr 2005 12:41:16 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Vladimir Igoshev <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="utf-8"
From:
Vladimir Igoshev <[log in to unmask]>
Parts/Attachments:
text/plain (182 lines)
Yes, after reflow.
Regards,
Vladimir
Sent from my Blackberry Wireless 
Vladimir Igoshev, 519-888-7465 ext.5283


-----Original Message-----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Fri Apr 29 12:17:00 2005
Subject: Re: [TN] gold vs copper plating on pcb's - Black PAD???

All,
How is to detect black pad? Can it be inspected at PCB
level? I guess no. Is it the after reflow soldering
phenomena?

Re,
Ken Patel


--- Werner Engelmaier <[log in to unmask]> wrote:
> Hi Bob,
> First, with ENIG you do not solder to gold, but to
> the underlying nickel;
> Second, soldering to Ni requires more thermal
> energy, thus higher temperatures, and that is really
> bad news on top of the T-increase necessary for
> LF-solders;
> Third, the 'black pad' issue will not go away with
> LF-solderas,but actually may become worse.
> Thus, Immersion Ag is a good choice.
> Werner Engelmaier
>
> -----Original Message-----
> From: Jeffrey Bush <[log in to unmask]>
> To: [log in to unmask]
> Sent: Wed, 27 Apr 2005 07:14:42 -0400
> Subject: Re: [TN] gold vs copper plating on pcb's
>
>
> If you stick with ENIG and do not test Immersion
> Silver then I am sure
> you will be doing future testing to combat the
> issues with ENIG.  Monies
> are being put into the development if silver and
> several toughed
> formulas are coming out that have excellent
> resistance to TC and do not
> have the issues associated with ENIG.  OSP is also
> seeing some
> development, but I do not see this as a viable
> alternative today.
>
> Jeffrey Bush
> Director, Quality Assurance and Technical Support
>
> VERMONT CIRCUITS INCORPORATED
>   76 Technology Drive - POB 1890
>     Brattleboro, Vermont 05302
>       Voice: 802.257.4571.21 Fax: 802.257.0011
>            http://www.vtcircuits.com
>
>
> -----Original Message-----
> From: Bob Arciolla [mailto:[log in to unmask]]
> Sent: Tuesday, April 26, 2005 4:41 PM
> To: [log in to unmask]
> Subject: [TN] gold vs copper plating on pcb's
>
> Good Afternoon all,
>
> Our company will be switching over to lead free and
> we have received
> sample pcb's from one of our vendors and one board
> has gold (ENIG) for
> the traces and one has copper (OSP). From some of
> the emails I have seen
> on Technet it appears that gold is what most of
> companies are going to
> be using? Is this correct or is there some other
> materials we should be
> looking into to use? Is the gold more reliable than
> the copper?
> Any input would be greatly appreciated.
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using
> LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask]
> with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of
> Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts:
> send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional
> information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100
> ext.2815
>
-----------------------------------------------------
> Regards, Bob
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using
> LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of
> Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts:
> send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or
> 847-615-7100 ext.2815
>
-----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using
> LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of
> Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts:
> send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
>
-----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------




---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2