Ofer
Does the supplier have any evidence of this corrosion? Over the past 10 years I have seen many immersion silver boards with plugged vias without any earmarks of corrosion.
Best regards
Lee
----- Original Message -----
From: Ofer Cohen<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Monday, April 04, 2005 10:59 AM
Subject: Re: [TN] Immersion Silver
Fellows,
I was just acknowledged by a PCB manufacturer that both ImAg and ImSn will be damaged if via holes are plugged (rather than tented). The ImAg will be corroded and the IMC layer of the ImSn will grow. As the plugging process (said he) is the very last process, both finishes will be Both will be polluted by the residues. His suggestion is to fill the vias before the external coating.
Did anyone meet the described problems?
Regards
Ofer Cohen
Manager
Quality Assurance, Reliability and Production Technologies
Seabridge Ltd. - A Siemens Company
Siemens COM FN A SB TQM
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|