April 3, 2005
Kester will no longer make HF1189 flux.
----- Original Message -----
From: Bill Kasprzak<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Friday, April 01, 2005 11:13 AM
Subject: Re: [TN] Heavy PCB Copper Wave Soldering...
Steve,
My approach on a board like this might include the use of a water based
water soluble flux like, HF-1189A. This way you can preheat your board in
an oven prior to wave then still apply flux without vaporizing it.
It'll be interesting to see how you handled these monsters. Keep us
posted. Good luck.
Bill Kasprzak
Moog Inc
Process Engineer, Electronic Assembly
Stephen Gregory <[log in to unmask]<mailto:[log in to unmask]>>
Sent by: TechNet <[log in to unmask]<mailto:[log in to unmask]>>
03/31/2005 05:41 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]<mailto:[log in to unmask]>>; Please respond to
[log in to unmask]<mailto:[log in to unmask]>
To
[log in to unmask]<mailto:[log in to unmask]>
cc
Subject
[TN] Heavy PCB Copper Wave Soldering...
Hi Ya'll!!
I just thought I'd share what is going to make things a little
more interesting for me here at work over the next couple
of days...
Go to: http://www.stevezeva.homestead.com<http://www.stevezeva.homestead.com/> and look at;
"Heavy Metal", Heavy Metal 2, and Heavy Metal 3. This
an assembly that I will be wave soldering, that has two 20-ounce
layers of copper on layers 2 and 11 (this is a 12-layer board).
I may be asking for some help for this...
My first try is to preheat and bake the assembly in a oven close
to the wave solder machine at 150 C., and then quickly remove
it from the oven, get it into the wave as soon as I can before it has
a chance to cool down, and see what kind of barrel fill I get.
I'll let you all know if this works, or I may be asking for some
help...
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc. It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>
for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|