Buehler, Ltd. has some useful technical information on their website
also.
http://www.buehler.com/emailcampaigns/default.asp?PagePath=:8080/publicl
ogin/login.aspx
Rich K / KEDS
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Parial Swati
Sent: Tuesday, April 12, 2005 12:51 AM
To: [log in to unmask]
Subject: [TN] Microsection for checking hole quality
Dear friends,
Are there any guidelines available regarding the microsections done for
checking the drill hole quality ? Any web sites or ipc document
reference will also be very helpful.
Thanks.
Warm regards,
Swati Parial
Scan by AT&S virus protection
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------