Phil
As already advised, silicone is the worst choice. My suggestion is an
acrylic unless NO out-gassing is allowed.
--
Regards Graham Naisbitt
[log in to unmask]
Golf quote of the week: If you watch a game, it's fun. If you play it, it's
recreation. If you work at it, it's golf.
Concoat Limited - Engineering Reliability in Electronics
A British Manufacturer
NEW WEB SITE: www.concoat.co.uk :NEW WEB SITE
Cell: 079 6858 2121
Office: +44 (0)1252 813706
On 21/3/05 11:40 pm, "DUTTON Phil" <[log in to unmask]> wrote:
> Hello,
>
> I've been asked what to use as a conformal coating for a high voltage
> circuit (<4kV).
> Also we want low out gassing because of some sensitive optical
> components.
> I'm thinking a silicone would be ok. Any advice would be welcome.
>
> thanks,
>
> Phil Dutton C.I.D.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|