Thanks Joe:
The time between first and second reflow is no more than 30 minutes.
Do you think that is enougth time to reabsorb moinsture ?
saul
>>> "Macko, Joe @ IEC" <[log in to unmask]> 3/10/2005 10:28:57 AM
>>>
Saul,
One of our contract manufacturer's has also seen this phenomenon. We
are
still trying to figure out the cause. What is the board's floor life
between 1st and 2nd side reflow? Maybe the PCB/BGA's are reabsorbing
moisture.
joe
-----Original Message-----
From: Saul MorenoRodriguez
[mailto:[log in to unmask]]
Sent: Wednesday, March 09, 2005 7:15 PM
To: [log in to unmask]
Subject: [TN] Voids
Hello Technetters:
In a recently running we had a problem with voids in Micro BGA's.
We resolved succesfully only increasing the preheat and the soak time,
this to dry the humidity correctly in the devices.
But my doubt is here:
The Micro BGA's are placed on first side and in first reflow we didn't
have problems,
all was ok, but voids showed up in the second reflow .
We detected them in 5DX.
Could you tell me why this happened ?
Thanks in advance..
Saul Moreno R.
Process Engineer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
_____________________________________________________________________________
Scanned by Sanmina-SCI eShield
_____________________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|