TECHNET Archives

March 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 7 Mar 2005 09:46:59 -0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Eric CHRISTISON <[log in to unmask]>
Subject:
From:
Eric CHRISTISON <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
<20050304165818.JJXQ21785.priv-edtnes46.telusplanet.net@JohnLaptop>
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (237 lines)
John,

I know something about plating but we are not a plating company.

The other thing I should have asked about is quantity.

The biggest difficulty you may have is plating selectively, especially if
the component is 3 dimensional. My experience with plating is of vacuum
deposition plating for EMC protection. We moved away from PC because it did
not give the best adhesion - however it may be OK for your customer's needs.
If you did go for a vacuum deposition process you'd have to arrange for
masking of the component in the same way that you would mask a component if
you painting it. This could be using some kind of tape or a fixture.

I also found that surface finish has only a second order influence on
adhesion. If you have good plating a smooth finish won't cause failure and
vice versa with poor plating. People plate plastic for mirrors and the
plastic substrate has to have a mirror finish...

Sorry I can't be more specific but hope this helps.

Regards,

Eric  Christison
Mechanical Engineer
Consumer & Micro Group - Imaging Division
STMicroelectronics
33 Pinkhill
Edinburgh
EH12 7BF

Tel:     +44 (0)131 336 6165
Fax:    +44 (0)131 336 6001


> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of John Parsons
> Sent: Friday, March 04, 2005 4:58 PM
> To: [log in to unmask]
> Subject: Re: [TN] Conductive Pattern on Lexan?
> 
> 
> With regards to Peters suggestion of silver deposition, I had 
> suggested that to them and I will mention it again.
> 
> Eric, your questions are all good, but I do not have that 
> information at this time.  Is your organization in such 
> things?  Should I hook up my customer with you directly?
> 
> John
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Eric CHRISTISON
> Sent: Friday, March 04, 2005 8:34 AM
> To: [log in to unmask]
> Subject: Re: [TN] Conductive Pattern on Lexan?
> 
> How big a component are they talking about and is it flat or 
> 3 dimensional?
> 
> Do they need good adhesion? What sort of environment is this 
> part destined for?
> 
> Regards,
> 
> Eric  Christison
> Mechanical Engineer
> Consumer & Micro Group - Imaging Division
> STMicroelectronics
> 33 Pinkhill
> Edinburgh
> EH12 7BF
> 
> Tel:     +44 (0)131 336 6165
> Fax:    +44 (0)131 336 6001
> 
> 
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
> > Sent: Friday, March 04, 2005 4:21 PM
> > To: [log in to unmask]
> > Subject: Re: [TN] Conductive Pattern on Lexan?
> > 
> > 
> > Lexan is GE's generic trade name for their polycarbonate
> > resin family, so there are various grades, probably one would 
> > be OK. A flex circuit manufacturer would be a good place to 
> > start talking as it is likely to be similar process to those 
> > used to make polymer circuitry.
> > 
> > Regards
> > 
> > Mike Fenner
> > Indium Corporation
> > 
> > T: + 44 1908 580 400
> > M: + 44 7810 526 317
> > F: + 44 1908 580 411
> > E: [log in to unmask]
> > W: www.indium.com
> > Pb-free: www.Pb-Free.com
> > 
> > 
> > 
> > 
> > 
> > 
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]] On Behalf Of John Parsons
> > Sent: Friday, March 04, 2005 4:00 PM
> > To: [log in to unmask]
> > Subject: [TN] Conductive Pattern on Lexan?
> > 
> > 
> > Happy Friday!
> > 
> >  
> > 
> > I have a customer who would like to produce a conductive
> > pattern, preferable with a gold finish on ½ to 1” thick Lexan 
> > or some other clear dielectric. Clear because they want to be 
> > able to see through it and the thickness will be required to 
> > withstand a significant pressure that will be on the surface. 
> > That is all the information I have at present.  
> > 
> >  
> > 
> > Any of you guru’s out there have any ideas/suggestions as to
> > either the feasibility or impossibility?  Offhand I don’t 
> > know if Lexan would stand up to the various processes in the 
> > regular PCB etching/plating processes.  Even suggestions as 
> > to another industry capable of this feat would be appreciated.
> > 
> >  
> > 
> > Regards
> > 
> > John Parsons
> > 
> >  
> > 
> > 
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV
> > 1.8e To unsubscribe, send a message to [log in to unmask] with 
> > following text in the BODY (NOT the subject field): SIGNOFF 
> > Technet To temporarily halt or (re-start) delivery of Technet 
> > send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at: 
> > http://listserv.ipc.org/archives Please visit IPC web site 
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> 
> :::::::::::::::::::::::::::
> 
> This email, its content and any files transmitted with it are 
> intended solely for the addressee(s) and may be legally 
> privileged and/or confidential. If you are not the intended 
> recipient please delete and contact the sender by return and 
> delete the material from any computer. Any review, 
> retransmission, dissemination or other use of, or taking of 
> any action in reliance upon, this information by persons or 
> entities other than the intended recipient is prohibited.
> 
> Messages sent via this medium may be subject to delays, 
> non-delivery and unauthorized alteration. This email has been 
> prepared using information believed by the author to be 
> reliable and accurate, but Indium Corporation makes no 
> warranty as to accuracy or completeness. In particular, 
> Indium Corporation does not accept responsibility for changes 
> made to this email after it was sent. Any opinions or 
> recommendations expressed herein are solely those of the 
> author. They may be subject to change without notice.
> 
> :::::::::::::::::::::::::::
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 
> 1.8e To unsubscribe, send a message to [log in to unmask] with 
> following text in the BODY (NOT the subject field): SIGNOFF 
> Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE 
> mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest Search the archives of 
> previous posts at: http://listserv.ipc.org/archives Please 
> visit IPC web site 
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
> additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 
> 1.8e To unsubscribe, send a message to [log in to unmask] with 
> following text in the BODY (NOT the subject field): SIGNOFF 
> Technet To temporarily halt or (re-start) delivery of Technet 
> send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: 
> http://listserv.ipc.org/archives Please visit IPC web site 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2