TECHNET Archives

March 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 18 Mar 2005 14:33:17 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (229 lines)
                I would solder suck most of the solder with a hot tip solder sucker or with solder wick then use them. I believe that it is cosmetic and the risk is minimum.
                Regards,
                Ramon
        	

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bill Kasprzak
Sent: Friday, March 18, 2005 2:13 PM
To: [log in to unmask]
Subject: Re: [TN] Solder on top of LCCC


Steve,

You've got the answers to your question.

Is this vendor willing to put the answer in writing?  If so, you are in
great shape.

Too often I've found vendors willing to bend but unwilling to put it
writing. In the age of suing everyone, who could blame them.

Bill Kasprzak
Moog Inc
Process Engineer, Electronic Assembly



Stephen Gregory <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
03/18/2005 01:56 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]


To
[log in to unmask]
cc

Subject
Re: [TN] Solder on top of LCCC






Hi Steve,

These are for a class-3 military application. This is a oscillator
M55310/19-BO3A40000
made by XSIS Electronics (they're out my way in Shawnee, Kansas).

I called them and they said they should be fine. The lid is welded with a
seam sealer and
there is no solder used, is what I was told.

-Steve Gregory-



|---------+---------------------------->
|         |           "Creswick,       |
|         |           Steven"          |
|         |           <SCreswick@GENTEX|
|         |           .COM>            |
|         |           Sent by: TechNet |
|         |           <[log in to unmask]>|
|         |                            |
|         |                            |
|         |           03/18/2005 10:13 |
|         |           AM               |
|         |           Please respond to|
|         |           TechNet E-Mail   |
|         |           Forum; Please    |
|         |           respond to       |
|         |           "Creswick,       |
|         |           Steven"          |
|         |                            |
|---------+---------------------------->

>--------------------------------------------------------------------------------------------------------------|
  |                                       |
  |       To:       [log in to unmask]  |
  |       cc:                                       |
  |       Subject:  Re: [TN] Solder on top of LCCC                |

>--------------------------------------------------------------------------------------------------------------|




Steve,

I would add a degree of caution here.  Many of the good ol' high temp
co-fired LCC's used gold-tin [80/20] for sealing of the lid to the
package.

If you immerse the gold-tin into normal tin bearing solder, eventually
your
package seal will be compromised.

I would lean to the side of WHAT your QA people are saying, but not
BECAUSE
of what they are saying and reject these units.   .... but then I do not
know what the application is either ...  Likely not to use them in Mil
product

Just my two bits

Steve C

-----Original Message-----
From: Stephen Gregory [mailto:[log in to unmask]]
Sent: Friday, March 18, 2005 10:46 AM
To: [log in to unmask]
Subject: [TN] Solder on top of LCCC


Happy Friday All Ya'll!!

We have some LCCC's that needed gold removal, and we did them here
in house manually. The lady that I had doing this was really careful, but
she
got some solder on top of a few of them.

QA was wanting to scrap them because of "solder contamination". I disagree
that they should be scrapped. I can't find any spec that says they need to
be
scrapped. You can still read the part numbers, and there are no solder
shorts
from the castellations to the top. Go to:

http://www.stevezeva.homestead.com

and look at "Solder on LCCC", and tell me what you think....these are
$50.00 ea.
and I don't want to scrap them if I don't have to.

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2