Ted,
You will find mil specs and the IPC specs in general agreement that most
conformal coatings should be applied in the range of 1-5 mils of thickness,
or 0.5 mils if you are using Parylene. If you start to go thicker than
this, you start to get problems arising from the cure dynamics (entrapped
solvents) which can result in poor adhesion, bubbling, that sort of thing.
Doug Pauls
Ted Kong
<zombietheking@YA
HOO.COM> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
03/17/2005 07:17 [TN] Conformal Coating
PM
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Ted Kong
<zombietheking@YA
HOO.COM>
Hi all,
We need to apply conformal coating to one of our
products. Is there a standard in the industry that
specify the material and the thickness? I guess Mil
Spec might have a standard out there, but don't know
what spec number. I would appreicate if someone
provide some guidelines or a spec number. Thanks all
in advance.
Ted
__________________________________
Do you Yahoo!?
Yahoo! Small Business - Try our new resources site!
http://smallbusiness.yahoo.com/resources/
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|