Bob,
Hmmm I am looking at a brochure of a reputable analytical company selling analytical XRF and it shows a clearly discernible Cd peak at ~150 ppm. BUT it does not say the collimator size. Certainly no bigger than 1 cm x 1 cm, which of course is too big for components. What size are you referring to?
Bev
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]]On Behalf Of Hilty, Robert D
Sent: March 15, 2005 9:01 AM
To: [log in to unmask]
Subject: Re: [LF] Site for Lead-Free Spot Tests
Correct, but you are not trying to achieve 1000 or 100 ppm accuracy with
these tests. XRF, such as those described below, is good for composition to
about 0.3% (3000 ppm) depending on collection time, standards, sample
geometry and equipment precision.
Bob
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]]On Behalf Of Wenger, George M.
Sent: Tuesday, March 15, 2005 8:03 AM
To: [log in to unmask]
Subject: Re: [LF] Site for Lead-Free Spot Tests
James,
We've been routinly measuring the plating thickness and composition of 0.5mm
pitch pads for years with our XRF which has a 3-mil collimator. We've also
correlated our measurements with Auger depth profiling so we know they are,
maybe not extremely accurate, but they are most certainly in the ballpark.
Regards,
George
George M. Wenger
Reliability / FMA Engineer
Base Station and Subsystems Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908) 546-4531
[log in to unmask]
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]]On Behalf Of Bev Christian
Sent: Tuesday, March 15, 2005 7:55 AM
To: [log in to unmask]
Subject: Re: [LF] Site for Lead-Free Spot Tests
James,
If this is the case, then how have we been able to use thickness XRFs for
years to measure plating thicknesses and the collimators are in the order of
12 mills in diameter?
Bev
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]]On Behalf Of James, Chris
Sent: March 15, 2005 3:39 AM
To: [log in to unmask]
Subject: Re: [LF] Site for Lead-Free Spot Tests
XRF's need around 1" sq surface area to work on which eliminates their
use on all components and most PCB's.
Regards,
Chris
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of MA/NY DDave
Sent: 15 March 2005 04:52
To: [log in to unmask]
Subject: Re: [LF] Site for Lead-Free Spot Tests
Hi Chris, IPC LF Listservers,
Forgetting the Spot Tests for a minute, how about these hand held XRF
units
that your links to SMART testing also found unreliable.
I just fast read, I believe the complete IEC test document 7x pages,
that
indicated that portable XRF units were fully acceptable.
GEE, Isn't this implementation phase FUN!!!
with lots of bumps on the road, Now don't groan...
Yours in Engineering, Dave
Y i Engr, MA/NY DDave
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
-----------------------------------------
This message (including any attachments) may contain confidential
information intended for a specific individual and purpose. If you are not
the intended recipient, delete this message. If you are not the intended
recipient, disclosing, copying, distributing, or taking any action based on
this message is strictly prohibited.
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
----------------------------------------------------------------------------
--------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
----------------------------------------------------------------------------
--------------------
[mf2]
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|