There may be some board manufacturers out there who can help me.
I'm currently trying to put an EMC shield on an component moulded in LCP. I
find that I can use a vapour deposition to do this but I get adhesion
failures because small areas of the top layer of the polymer delaminate from
the bulk of the moulding.
When LCP is plated in PCB substrates does the same problem occur or is the
delamination being caused by the deposition process damaging the substrate?
What is the normal plating recipe in the PCB industry for LCP anyway and
what adhesion test would be specified?
Regards,
Eric Christison
Mechanical Engineer
Consumer & Micro Group - Imaging Division
STMicroelectronics
33 Pinkhill
Edinburgh
EH12 7BF
Tel: +44 (0)131 336 6165
Fax: +44 (0)131 336 6001
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------