Been out and have trouble untangling the 2 parallel threads, so I gave up.
My apologies if I duplicate responses.
Are you vapour cleaning after the first print? If the first clean was not
complete, cleaning a twice baked reside will be harder and even less
complete and could easily show as a white residue.
Are there any other fluxes on board, like a wave solder flux? Or hand
touch-up flux? This will often show like this.
Regards
Mike Fenner
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blomberg, Rainer (FL51)
Sent: Thursday, March 10, 2005 3:21 PM
To: [log in to unmask]
Subject: Re: [TN] Cleaning residues off of PCB
Jason,
I have seen similar results during cleaning process evaluations. In my
case, clear residue was residual flux that remains in the small spaces
common to fine-pitch parts after the cleaning solvent has evaporated. You
might be seeing the Non-volatile Residue. Evaporation is slowest in the
small spaces, especially between solder pad and solder mask. In addition,
capillary forces will draw and hold liquid there making it slow to
evaporate. This was solved by longer cleaning time (to get more flux off)
and better rinsing/drying to rinse away the "dirty" flux removing solvent
and get rid of the NVR.
I am surprised that your vapor degreasing process alone is not adequate to
get rid of flux residue. The vapors should penetrate and get to all
surfaces. Either the part is in vapor too short a time or you are seeing
residue left by the secondary wash/rinse in "contaminated" terpene.
We use Kyzen Ionox I3330 at 140 deg. F followed by a clean Isopropyl alcohol
spray rinse. Without the clean IPA rinse, our boards would look like yours.
Hope this helps,
> Rainer G. Blomberg
> Staff Production Engineer
> Space Systems - Clearwater
> Honeywell International, Inc.
> * Phone (727) 539-5534
> * Fax (727) 539-4469
> * Email [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Gregory
Sent: Wednesday, March 09, 2005 6:37 PM
To: [log in to unmask]
Subject: Re: [TN] Cleaning residues off of PCB
Photo posted. Thanks Steve!
You can see (barely - sorry bad photo) some halo-ing around the leads. Like
I said, no other detection in open areas or two leaded devices just finer
pitch, multi-leaded devices.
Follow the link
http://www.stevezeva.homestead.com/files/residue_closeup.jpg
Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)212-0844 cell
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of David D. Hillman
Sent: Wednesday, March 09, 2005 4:05 PM
To: [log in to unmask]
Subject: Re: [TN] Cleaning residues off of PCB
Hi Jason! Can you send a photo to Steve for posting? A visual would help.
Dave Hillman
Rockwell Collins
[log in to unmask]
Hello all,
We have some boards that I am requiring some advice on cleaning residues.
The PCBs were soldered with SN96 (Sn96.5/Ag3.5). The first pass of the
boards look great. However, the second pass looked very suspicious. We are
seeing residue that looks like dried, puddled flux residue around most of
the leads. The areas mostly affected are multi-leaded components and there
is no evidence of this residue in open (non-populated) areas of the board.
If we take something like a probe or tweezers and move them along the areas
of concern, then it flakes off, but not real easily. I am afraid to do this
in fear of damaging the laminate (these are expensive boards). We have tried
re-fluxing them with aggressive RMA flux and re-reflowing them, but to no
avail. I have just tried soaking them, for 15 minutes, in a 50/50 solution
of distilled white vinegar and DI water, but again, to no avail.
Does anyone have any suggestions as to something else to use that's
aggressive, but not damaging to polyimide (or the solder joints)?
TIA,
Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)212-0844 cell
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
:::::::::::::::::::::::::::
This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.
:::::::::::::::::::::::::::
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|