Steve,
It well may be a surface contamination/cleanliness issue (prior to plating).
Vladimir
Vladimir Igoshev, Ph. D.
Senior Materials Researcher
Research in Motion
451 Phillip St.
Waterloo, ON, N2L 3X2
Voice: (+1) 519-888-7465, ext. 5283
Fax: (+1) 519-886-0863
E-mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Stephen Gregory
Sent: Monday, March 07, 2005 11:11 AM
To: [log in to unmask]
Subject: [TN] Peeling Plating...
YAY! IT'S MONDAY!!! YAY!
(Ya'll are probably saying; "Sheesh, what's Steve been smoking?")
I'm not smoking anything...I said "YAY" with my tongue in my cheek, so to
speak.
It's Monday again, and I have a couple of pictures for you to look at and
let me know
if any of you have seen anything like this before. We got these pictures
from our customer
asking us if we know what might have caused this. Go to:
http://www.stevezeva.homestead.com
and look at "Plating Peel" and "Plating Peel Close-up". Obviously, this is
something that
you don't want to see on component leads. It kinda' looks like the lead is
shedding it's
skin...
We're going to contact the component vendor about this to see if they can
shed some light
on why this is happening...I wished I had the assembly here that the
pictures came from, but
we only have the photos right now.
Anybody ever seen this before?
"Monday, monday...can't trust that day
Monday, monday...sometimes it just turns out that way
Oh monday mornin' you gave me no warnin' of what was to be
Oh monday, monday...how could you leave and not take me."
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc. It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|