As far as I know, there is no universal lead-free solder being used. Won't
there be complications with mixing alloys.
The manufacturers of the solder leveling lines might like it but I can just
see what happens when someone proposes we need to buy multiple lines to run
different alloys.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete Lymn
Sent: Wednesday, March 30, 2005 7:06 AM
To: [log in to unmask]
Subject: Re: [TN] Lead free solder HAL
Done correctly it looks just as bright as good SnPb Russ. The 'colour' is
slightly different and varies a little with the alloy of choice. In general
you will find the maximum thicknesses (small features) will be thinner and
the minimum thicknesses (ground areas) thicker. You tend not to see that
'air swept' look on earth plains. Hole clearing is better.
Done incorrectly its looks ugly! The operating window is narrower (your
operating with very little super heat) As the copper content increases or
the solder temperature drops the copper will separate from the tin leaving
you with dull gritty dendritic deposits...
Nothing solders like solder. We have never had a board returned for
solderability problems but we re process lots of other 'alternative' surface
finishes.
I don't see it Is a new process, its just a different alloy.
-----Original Message-----
From: Russell Burdick [mailto:[log in to unmask]]
Sent: 30 March 2005 03:04 PM
To: [log in to unmask]
Subject: Re: [TN] Lead free solder HAL
What should the surfaces cosmetically look like off the solder free HAL
machine? Bright and shiny as our HASL? If not, what is the indicator that
quality-wise the process is nearing the edge of acceptability?
Are your customers well versed in the assembly of boards with the lead free
solder finish? What types of solderability issues might I encounter if a
customer has difficulty and "suspects" that it is a board problem compared
to an assembly problem? (there is always a money aspect to every
situation...)?
I do understand that as a new process competing with an established one it
will garner its own implementation issues. Operators could unwittingly apply
the known guidelines of HASL and resist the new process as "not like the
good old stuff".
Russ
>From: Pete Lymn <[log in to unmask]>
>Reply-To: TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
>To: [log in to unmask]
>Subject: Re: [TN] Lead free solder HAL
>Date: Wed, 30 Mar 2005 14:38:26 +0100
>
>We have been working with lead free alloys in HASL machines since '98
>and have been leveling panels commercially for about 5 years. What
>would you like to know?
>
>-----Original Message-----
>From: Russell Burdick [mailto:[log in to unmask]]
>Sent: 30 March 2005 01:19 PM
>To: [log in to unmask]
>Subject: [TN] Lead free solder HAL
>
>
>Good Morning Technet,
>
>I am at the early stages of learning about lead free solder as an
>alternative option to our current tin/lead solder HASL.
>
>Is there anyone out there who can comment about their experiences?
>
>Currently I have no customers requesting this process, but I need to be
>ahead of this need when feasible.
>
>Vendors have provided both sides, yes PCB makers are doing it and a
>large PCB maker tried it and discontinued using it.
>
>Thanks in advance.
>
>Russ Burdick, trying to lessen the HASL hassle
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>or
>(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
>NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
>e-mail to [log in to unmask]: SET Technet Digest Search the archives of
>previous posts at: http://listserv.ipc.org/archives Please visit IPC web
>site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|