We have been working with lead free alloys in HASL machines since '98 and
have been leveling panels commercially for about 5 years. What would you
like to know?
-----Original Message-----
From: Russell Burdick [mailto:[log in to unmask]]
Sent: 30 March 2005 01:19 PM
To: [log in to unmask]
Subject: [TN] Lead free solder HAL
Good Morning Technet,
I am at the early stages of learning about lead free solder as an
alternative option to our current tin/lead solder HASL.
Is there anyone out there who can comment about their experiences?
Currently I have no customers requesting this process, but I need to be
ahead of this need when feasible.
Vendors have provided both sides, yes PCB makers are doing it and a large
PCB maker tried it and discontinued using it.
Thanks in advance.
Russ Burdick, trying to lessen the HASL hassle
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|