Phil:
You will probably want to try Chris Schaefer's ideas first, as they sound relatively benign, but if the problem really is Tin oxide, I suspect they may not work, but I have something that will. It is very very alkaline, but is like a silver bullet for Tin oxide.
Contact me off Technet for further information.
Rudy Sedlak
RD Chemical Company
[log in to unmask]
650-962-8004
Phil Nutting <[log in to unmask]> wrote:
Gee, it would be great to come up with something for my closed loop DI
batch washer.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Schaefer, Chris
Sent: Tuesday, March 22, 2005 4:17 PM
To: [log in to unmask]
Subject: Re: [TN] In-Line Washer De-scaling.
Scott,
We typically use in our water wash a Kester 926 de-scaler (5 gl./ 60 gl.
tank) with 2 gallons of vinegar . Now if has been a while and the scale
if very difficult to remove we use a Kyzen A4512P (10% concentration),
which will remove pretty much anything that we have come across. Now in
our No-Clean wash we use the Kyzen A4512P to remove ALL residues, so we
do not de-scale - - - EVER! I believe I have the cleanest machine
around. Anyhooo! I hope this helps.
Chris Schaefer
Process Engineer
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Scott Lefebvre
Sent: Tuesday, March 22, 2005 2:11 PM
To: [log in to unmask]
Subject: [TN] In-Line Washer De-scaling.
Can anyone recommend some type of De-scaler product for our in-line
washer. We have been accumulating a white powdery substance which I
understand is a by product of the Kester 2224-25 Flux.
Scott
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
__________________________________________________
Do You Yahoo!?
Tired of spam? Yahoo! Mail has the best spam protection around
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
http://mail.yahoo.com
|