TECHNET Archives

March 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 18 Mar 2005 15:49:31 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Roger Stoops <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Roger Stoops <[log in to unmask]>
Parts/Attachments:
text/plain (230 lines)
Neat chart...
http://www.redpulsar.us/~coldfusion/freeze.html


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Precision Analytical
Lab
Sent: Friday, March 18, 2005 3:34 PM
To: [log in to unmask]
Subject: Re: [TN] Answer to Friday's question

It has to do with the total number of particles in solution.  In this
case, the smaller the number, the faster it freezes..and vice versa.  I
begin with the same weight of material, 10 grams, but I have to take
each formula weight into account as well.

Popsicles also have other ingredients, such as flavorings, etc.
Anti-freeze has methanol along with the glycol to help lower it's
freezing point.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bill Kasprzak
Sent: Friday, March 18, 2005 3:17 PM
To: [log in to unmask]
Subject: Re: [TN] Answer to Friday's question


I disagree.

Why do Popsicle's stay frozen in my freezer while the anti freeze in my
car is protects my car to 20 below F.

Certainly my freezer doesn't go to 30 below F.

Now I know why I'll get a bloody nose.

Bill Kasprzak
Moog Inc
Process Engineer, Electronic Assembly



Precision Analytical Lab <[log in to unmask]> Sent by:
TechNet <[log in to unmask]>
03/18/2005 02:37 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to Precision
Analytical Lab <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Answer to Friday's question






Alright,

First of all, that much sucrose or calcium chloride will not completely
dissolve in that little of DI water.  So, the original question was a
tad bit on the devious side.

However, if you did use enough DI water to completely dissolve each of
those materials, they will begin to freeze in this order:  First to
begin freezing is the ethylene glycol (antifreeze), second will be the
calcium chloride (Indiana's road salt), and last is the sucrose (sugar).

Happy Friday!

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Graham Naisbitt
Sent: Friday, March 18, 2005 1:04 PM
To: [log in to unmask]
Subject: Re: [TN] Friday question


Shawn

You are what we call over here, a real stinker! Its Friday and I am not
less than 5 hours ahead of all you guys and now I will have to spend the
entire week-end wondering about the true answer.

My shot will be Calcium Chloride time because of the De-ionised water,
then sucrose unless the water is hot, then the diluted anti-freeze. I
haven't a clue as to why, just gut feeling.
--
Regards Graham Naisbitt

[log in to unmask]

Golf quote of the week: If you watch a game, it's fun. If you play it,
it's recreation. If you work at it, it's golf.

Concoat Limited - Engineering Reliability in Electronics A British
Manufacturer

NEW WEB SITE: www.concoat.co.uk :NEW WEB SITE

Cell: 079 6858 2121
Office: +44 (0)1252 813706




On 18/3/05 1:38 pm, "Precision Analytical Lab"
<[log in to unmask]> wrote:

> This one's real fun.  It's sure to make blood shoot out your nose.
>
> Which of these 3 solutions will freeze first, second, and third and 
> WHY
will
> they freeze in that order????
>
> 1) 10 grams of Calcium Chloride (road salt) dissolved in 20 mL of DI
water.
>
> 2) 10 grams of Sucrose (table sugar) dissolved in 20 mL of DI Water.
>
> 3) 10 grams of Ethylene Glycol (antifreeze) dissolved in 20 mL of DI
water.
>
>
> Shawn Parson
>
> Precision Analytical Laboratory
> 4106 Cartwright Drive
> Suite A
> Kokomo, IN  46902
> Ph: (765) 455-1993
>
> Specializing in Ion Chromatography (IC) and Surface Insulation
Resistance
> (SIR)
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To 
> unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing 
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
> additional information, or contact Keach Sasamori at [log in to unmask] or

> 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2