Delrin is a difficult plastic to get anything to adhere to, as it is a
"waxy" plastic. You might have some success with a two-part epoxy. I would
recommend scuffing the surface of the Delrin before gluing.
Dave Roach
Trane GCC
4833 White Bear Parkway
St. Paul, Minnesota 55110
651-407-4294
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chad Haima
Sent: Tuesday, March 01, 2005 11:53 AM
To: [log in to unmask]
Subject: [TN] Help!!
Anybody have some recommendations for glueing delrin and stainless steel
together. We're going through loctite and are getting nowhere. Any
help is much appreciated.
Thanks,
Chad Haima
Pentagon EMS
Ph: 503-924-2747
Fx: 503-924-2744
[log in to unmask]
www.pentagon-ems.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|