Have you considered lead free hasl?
-----Original Message-----
From: Matthew Lamkin [mailto:[log in to unmask]]
Sent: Tuesday, February 15, 2005 2:57 PM
To: [log in to unmask]
Subject: Re: [TN] OSP process for PCB
Special applications such as?
I have the task of coming up with the lead free finishes that we are going
to use. OSP will NOT be one of them (I have been told not to use it).
Changing to lead free has removed a few PCB suppliers from our lists.
Thank you,
Matthew Lamkin.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of George Milad
Sent: Tuesday, February 15, 2005 2:48 PM
To: [log in to unmask]
Subject: Re: [TN] OSP process for PCB
Immersion Tin is in use as a surface finish for specific applicatios, it is
not classified as an OSP (organic solderability preservative). Some common
OSPs are Benzotriazoles, Immidazoles and Benzimidazoles. they are non
metallic, organic compounds. Hope this is helpful.
Best regards
George Milad
[log in to unmask]
National Accounts Manager for Technology
Uyemura International Corporation
Technical Center
240 Town LIne Rd
Southington CT 06489
(516) 901 3874 (mobile)
(860) 793-4011 (office)
(860) 793-4020 (fax)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|