Hi Steve,
The symmetry looks okay.
However, my opinion, there's either trouble or cost or both in the copper
weights and possible core/pre-preg stacks.
Looks like getting the copper weights is the challenge.
If impedance is a key factor then there may be fun in getting equal resin
contents.
Assuming the 0.8mil is resist then:
1- 1.5oz
8.5mil Pre-preg.
2- 1oz
3 mil core, double copper
needs all the support it can get, hopefully between 2 planes! Okay for
copper so far
3- 1oz
12mil pre-preg, made of say a 2116/7628
4- 0.5oz
12 mil core -
could possibly be a sandwich of 2 single sided cores and a pre-preg to
ease availability of cores with right copper
5- 1oz
4mil pre-preg
6- 0.5oz
6mil core - double copper
Etc. repeated symmetrically
Best Regards
David Greig
______________________________
GigaDyne Ltd
Buchan House
Carnegie Campus
Dunfermline KY11 8PL
United Kingdom
t: +44 (0)1383 624 975
______________________________
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stephen Gregory
Sent: 25 February 2005 18:54
To: [log in to unmask]
Subject: [TN] Manufacturability of PCB Stack-up...
Happy Friday All!
I've posted a drawing of a PCB layer stack-up at:
http://www.stevezeva.homestead.com/files/Stackup.jpg
I'd like to verify its manufacturability. The reason for the verification
is that there are dielectric thicknesses that vary quite a bit from layer to
layer.
Can anybody comment on this?
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc. It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver this
message to anyone. In such event, you should destroy the message and kindly
notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
--
Virus scanned by Lumison.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|