Mr. Pitarys:
It is my understanding that there are two types of restrictions with RoHS, perhaps restrictions is too strong a term... one class is restricted, the other simply must be "registered", or noted, but I am not clear with whom.
Since cleaning chemicals wash away, and do not become part of the finished part, no chemicals are "restricted", and cannot be used.
However, if any chemicals on the RoHS are used in cleaning, they must be noted, and "registered", but may be used, since they are not part of the shipped component.
My belief is that you must ask your chemical vendors if their cleaners contain ingredients on the RoHS list. (And of course, get letters certifying that they do not.)
Rudy Sedlak
RD Chemical Company
Charlie Pitarys <[log in to unmask]> wrote:
Greetings! Is there a list of approved and non-approved cleaning
chemicals for this specification? Are cleaning chemistries involved if
at all? I found perhaps 10 compounds (mostly metals) and the rest of the
spec seems pretty vauge.(re. massive Google Search)
Is there a standard form to present to customers that your products are
in compliance or is it just a blanket faith statement?
Thanks in advance.
Charlie Pitarys
Director of Application Technologies
603.622.2900 x-115
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
Do you Yahoo!?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Read only the mail you want - Yahoo! Mail SpamGuard.
|
|
|