Sorry, no dendrites are a surface electrochemical thingie. What I'm
talking about is a kind of electrophoresis. :)
Brian
Johnson, Joseph wrote:
> Brian, You are right in all aspects of your explanation!
>
> Also the name of this migration that you are talking about I believe is
> called "Dendrites" (I probably have it spelled wrong...). I have seen
> photo's of traces actually growing conductive whiskers. This is another
> reason to space your low voltage traces as specified. This way you don't
> start to get a lot of field failures after 5-7 years.
>
> Joe J.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
> Sent: Thursday, February 03, 2005 4:32 AM
> To: [log in to unmask]
> Subject: Re: [TN] Technical basis for Table 6-1 of IPC-2221
>
> Your surmise may be partially true if you had FR-4 between the conductors,
> but you don't, you have air, and often humid air, at that.
> When I was a student, I was given a rule of thumb that humid air broke down
> (i.e. ionised) at a gradient of 15,000 V/inch (600 V/mm). Does that tell you
> anything? Of course, this rule of thumb is not a scientific absolute as
> there are many more variables, such as air pressure (altitude), temperature,
> relative humidity and, in the case of semi-planar devices such as PCBs,
> surface contamination.
>
> However, it doesn't even end there. FR-4 contains molecules of sodium
> chloride which "attract" humidity and can therefore ionise under the
> influence of a voltage gradient, and migrate within the resin matrix.
> This is measurable at gradients as low as 5 V/mm and can cause all sorts of
> funny effects at very high impedances, and it can "remember" its history
> over hours, because the fields between the positive and negative ions (after
> the causal gradient is removed) are so low that the reverse migration is
> very slow. I described this phenomenon in papers published in the second
> half of the 1980s and I also adjudicated the dissertation of a student at
> the Swiss Federal Institute of Technology who studied this phenomenon.
> Because of this, I recommended a max gradient of 100 V/mm for critical
> tracks on circuits working up to 10 megohms impedance, down to 5 V/mm at the
> order of a teraohm.
>
> Brian
>
> - Bogert wrote:
>
>>February 2, 2005
>>
>>Table 6-1 defines minimum electrical spacing requirements between traces
>
> on a PWB. What is the technical basis for the Table? Is there a formula
> associated with the values in the table? For example, if I have a PWB
> operating at 30 volts DC, the minimum spacing required between internal
> traces is 0.05 mm. What if a PWB operates at 30 VDC but only has 0.04 mm
> spacing, is there a technical concern? Based on what formula or technical
> consideration?
>
>>The minimum spacing in the Table are much less than the electric strength
>
> requirements for FR4. For example, my understanding is that FR4 is about
> 1250 volts/mil. Therefore, at 1 mil of spacing the PWB should be able to
> withstand 1250 volts between conductors.
>
>>The values in the table are also different than those included in UL 840.
>
> Why?
>
>>Any help you can offer on this point would be appreciated.
>>
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>>unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>>or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>>Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>>posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>>archives of previous posts at: http://listserv.ipc.org/archives Please
>>visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>for additional information, or contact Keach Sasamori at
>>[log in to unmask] or 847-615-7100 ext.2815
>>-----------------------------------------------------
>>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
> e-mail to [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please visit IPC web
> site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|