Scott:
The lead in glasses used in electronic components is exempt from RoHS
according to Annex Item 5
5. Lead in glass of cathode ray tubes, electronic components and fluorescent
tubes.
The glaze and resistive element in chip resistors in a typical lead
borosilicate glass. The conductor (in your MSDS) is ruthenium oxide - the
amount mixed into the glass determines the resistance value.
Cheers,
Dick Anderson - 978-442-5165
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Kallin, Dan
Sent: Thursday, February 24, 2005 4:49 PM
To: [log in to unmask]
Subject: Re: [LF] Lead Free Material Composition
It seems that each layer would be a homogenous material so that would be
your point of compliance.
It is the lead you are worried about, so if close, you would need to
calculate the amount of lead rather than PbO, however it seems this would
not be a problem even if it was lead at the percentages given.
This assumes the definitions and de minimus levels going back and forth get
finalized.
That is my opinion only, which, with a couple of bucks, will get you a
coffee.
Dan
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]]On Behalf Of Scott Lefebvre
Sent: Thursday, February 24, 2005 3:45 PM
To: [log in to unmask]
Subject: [LF] Lead Free Material Composition
I received a material composition datasheet from a manufacturer and I was
hoping if someone could review this pdf file. I noticed for some it's
component composition they are still using Lead Oxide. If lead oxide is
considered the same as Lead per ROHS then the permissible values given seem
to be above .1% wt total.
Just in case the PDF doesn't go through I'll provide some of the details.
Coating layer: Lead Oxide 0.87 wt%, Silicon dioxide 0.69 wt%, Boron
Trioxide 9.34 wt%, Aluminum 0.18% and ...
Resistive Layer: Lead oxide 0.30 wt%, Silicon dioxide 0.11 wt % and ......
Scott Lefebvre
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|