FR4 has been punched for years. I first worked in Asia in 1985 and worked in
Asia for over 14 years. Almost all of work is punched except for
multi-layers because of the fracturing between layer concern. If the
supplier has good controls they count the number of hits and resharpen the
tools. Layer count, board thickness and dimensional tolerance should dictate
to them if they can use a punch press or not.
Scott Westheimer
----- Original Message -----
From: "Greaves, Bernie (IMP)" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, February 16, 2005 10:54 PM
Subject: [TN] Cracking FR4
Hopefully someone in the forum may have had experience with cracking
along edge of FR4 as per attached photo. The profile of this pcb was
punched and subsequently the edge has fine cracks through the soldermask
and glass. We have had a large quantity of this part made in China and
are concerned that this cracking could compromise the board function.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|