Content-Type: |
text/plain; charset="iso-8859-1" |
Sender: |
|
Subject: |
|
From: |
|
Date: |
Wed, 2 Feb 2005 09:01:36 +0100 |
MIME-Version: |
1.0 |
X-To: |
|
Reply-To: |
|
Parts/Attachments: |
|
|
You are OK, relaxed and fine, Steve?
Enjoying life and planning the future?
Good.
How's the chat with Paul? He seems to be quite invisible at the moment.
Adding pic for your souvenir boutique.
Have a nice day..
Inge
-----Original Message-----
From: Ingemar Hernefjord (KC/EMW)
Sent: den 2 februari 2005 08:57
To: 'TechNet E-Mail Forum'; 'Zweigart, Siegmund'
Subject: RE: [TN] ENIG - Failures
Interesting. Why just few nanometers? We found that 0.5 to 1.5 um seemed to be quite normal.
I'll ask Mountain Jack to hang a skin on the wall. Not perfect a pic, but quite readable. In
this case, Xilinx helped me, their specialists are VERY skilled.
Ingemar Hernefjord
Ericsson Microwave Systems
PS. Steve, ready?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Zweigart, Siegmund
Sent: den 1 februari 2005 15:12
To: [log in to unmask]
Subject: [TN] ENIG - Failures
Hello all
We see the following issue on an ENIG coated PCB (soldered with SnPb):
After reflow solder joint is ok but cross section shows a quite irregular
IMC phase (about 3 mikrometer thick, not homogenous, looks more like stones
on a plane)
After the following wave process (component is on the top side) solder joint
is very fragile and in the cross section some fractures are seen.
Has somebody any picture how a perfect IMC on ENIG should look like? I would
expect a homogeous layer just a few nm thick.
Any ideas?
Siggi
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|