TECHNET Archives

February 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Genny Gibbard <[log in to unmask]>
Date:
Fri, 18 Feb 2005 11:18:14 -0600
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Genny Gibbard <[log in to unmask]>
Parts/Attachments:
text/plain (41 lines)
I have definitely seen better responses out of SOT86 and SOT89 pkgs when the
ground leads are resoldered in RF applications, but then often the layout
tends to have ground vias very close that may rob solder volume.  I don't
know if this applies in the SC79 situation or not.

-----Original Message-----
From: Karen Walters [mailto:[log in to unmask]]
Sent: February 18, 2005 11:00 AM
To: [log in to unmask]
Subject: Re: [TN] SC79 packaging


I would like to add a side note.  Parts on board when soldered do meet
IPC-610 criteria.

                      Karen Walters


Question:   Customer is stating they get better yield at test when the
solder extends to almost the body package of a SC79 package.  As the part
is designed this would not have any impact on part performance.  What I
believe is happening is when they resolder the part lead is making better
contact with the pad.

Have any of you had an issue with this package type that you had better
output responses when you added more solder/ reheated it up so that you can
get better output.  What did you do to improve the situation.  I believe it
is a solder reflow issue in the furnace while cooling.  Please advise.

Thanks

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2