What about Federal Specification QQS-571?
-----Original Message-----
From: Leland Woodall [mailto:[log in to unmask]]
Sent: Friday, January 21, 2005 6:26 AM
To: [log in to unmask]
Subject: [TN] Lead-free Wave Solder Pot Impurity Levels
Hi Folks,
I have a small dilemma here. There is a standard for eutectic solder pot
impurity levels, but I can't seem to find one for lead-free. Is there
such an animal?
Everything I've researched on the Web shows only recommendations, namely
from Alpha and AIM. Those two have slight disagreements.
At least they provide something, and that is impressive.
It also appears that the major concern is processing problems versus
product reliability. If copper content gets too high, the wave solder
viscosity becomes too high and bogs down the mechanical parts of the
machine.
When things get out of whack, can I expect reliability problems as well?
What levels of impurities would cause premature joint failure,
specifically?
Are we too new to this, and have tests not yet been agreed upon? Is IPC
addressing the issue?
Any help you could provide would be sincerely appreciated.
Offline comments are welcomed.
Many, many thanks,
Leland Woodall
Quality Coordinator
Keihin Carolina System Technology, Inc.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|