"Thermal" conductivity or "electrical" conductivity?
David A. Douthit
Manager
LoCan LLC
====================
Dehoyos, Ramon wrote:
> The relative conductivity of Copper is about twice that of aluminum.
> Regards,
> Ramon
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of Denis Lefebvre
>Sent: Thursday, January 13, 2005 2:25 PM
>To: [log in to unmask]
>Subject: Re: [TN] Aluminum substrates... any issues?
>
>
>I've heard of "copper core" boards before, but not aluminum. I suppose it would preferable with respect to the fact that aluminum is a better conductor than copper.
>
>-----Original Message-----
>From: Brooks,Bill [mailto:[log in to unmask]]
>Sent: Thursday, January 13, 2005 11:08 AM
>To: [log in to unmask]
>Subject: [TN] Aluminum substrates... any issues?
>
>
>I ran across this supplier of aluminum boards and was interested if any of
>you have dealt with this type of thing before? I have seen metal core boards
>made with alumina and bonded with the fiberglass/epoxy for heat sinking
>needs but this looks like a different process. Possibly less expensive...
>???
>
>http://www.irctt.com/pdf_files/thickfilm_aluminum.pdf
>
>Any comments on it are appreciated.
>
>Best regards,
>
>Bill Brooks - KG6VVP
>PCB Design Engineer , C.I.D.+, C.I.I.
>Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
>e-mail:[log in to unmask]
>http://www.dtwc.com
>http://pcbwizards.com
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|