Which end up where at end of life?
Given that lead in electronics (excluding CRT's) amounts to 0.5% of that
used globally one must question the ethics of imposed change.
The good thing for electronics will be stronger solder joints (if there made
at all!).
Downsides:
Equipment, and indeed companies, forced redundant by the change.
Increased energy used as a result of higher nitrogen usage and higher
temperatures.
Making solder from elements much less prevalent than lead.
Our beloved tin whiskers causing foreshortened reliability.
Etc.
Depending on where you are in the world, chances are that there is already
more lead in the ground soil that would ever get there via landfill
electronics.
Seems like an awful lot of energy and entropy for little gain. Quite typical
of Europe.
Best Regards
David Greig
______________________________
GigaDyne Ltd
Buchan House
Carnegie Campus
Dunfermline KY11 8PL
United Kingdom
t: +44 (0)1383 624 975
http://www.gigadyne.co.uk
______________________________
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hughes, Chris
Sent: 17 January 2005 16:52
To: [log in to unmask]
Subject: Re: [TN] Markings for Pb Free....
Lead is likely to be a viable material for equipment exempt from the RoHS
Directives and such like.
-----Original Message-----
From: David Greig [mailto:[log in to unmask]]
Sent: 17 January 2005 16:47
To: [log in to unmask]
Subject: Re: [TN] Markings for Pb Free....
Which reminds me -
Given that lead ores are often by-products of the tin mining industry, and
that tin, antimony, bismuth etc are by-products of lead extraction, what's
going to happen to all that unwanted lead when we still mine tin etc for
solder?
Land fill?
Best Regards
David Greig
______________________________
GigaDyne Ltd
Buchan House
Carnegie Campus
Dunfermline KY11 8PL
United Kingdom
t: +44 (0)1383 624 975
http://www.gigadyne.co.uk
______________________________
-----Original Message-----
From: David Greig [mailto:[log in to unmask]]
Sent: 17 January 2005 16:38
To: 'TechNet E-Mail Forum'; 'Rodney Miller'
Subject: RE: [TN] Markings for Pb Free....
http://www.ipc.org/TOC/IPC-1066.pdf free download, covers it, bit I've seen
some regional logo's elsewhere.
Best Regards
David Greig
______________________________
GigaDyne Ltd
Buchan House
Carnegie Campus
Dunfermline KY11 8PL
United Kingdom
t: +44 (0)1383 624 975
http://www.gigadyne.co.uk
______________________________
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rodney Miller
Sent: 17 January 2005 14:48
To: [log in to unmask]
Subject: [TN] Markings for Pb Free....
No standards or where to put them.
I don't know if 610 will cover it, but anybody putting it in PCB art, if so,
what?
Rodney L. Miller, CID
VP / Director of Manufacturing
Tri-onics Inc.
ph (618) 654-9831
fx (618) 654-6122
e [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
--
Virus scanned by Lumison.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
--
Virus scanned by Lumison.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|