Some use big N2 packs, which we used also in the beginning, but leasing a LN2 tank is much cheaper. Guess distance to LN2 producer decides. Nearly all atmosphere around this planet is N2, and we have to pay.... /Ingemar
PS. 73% Nitrogen and 26% Oxygen and a few secret gasses...that's earth atmosphere..I hope it's still free to breathe without license. Nearly missed the joke.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]
Sent: den 14 januari 2005 13:40
To: [log in to unmask]
Subject: Re: [TN] Must we applied N2 to reflow when using Pb-free solder
paste?
We do not do lead free right now but we do use a proprietary gas mix of
Approx. 73% Nitrogen and 26% Oxygen with a few other secret gasses in the
mix. I am sure we can work out a licensing agreement.
-----Original Message-----
From: Hughes, Chris [mailto:[log in to unmask]]
Sent: Friday, 14 January 2005 2:35 AM
To: [log in to unmask]
Subject: Re: [TN] Must we applied N2 to reflow when using Pb-free solder
paste?
Lee.
Very interesting.
Christopher Hughes
Environmental Scientist
[log in to unmask]
Statement of Confidentiality The document transmitted by this e-mail
contains information from Mabbett & Associates Ltd and its affiliates,
holdings or entities and may contain confidential and privileged information.
This information is intended for the use of the addressee named on this
transmittal sheet. If you are not the addressee, any disclosure,
photocopying, distribution, dissemination or use of its contents is strictly
prohibited. If you have received this e-mail in error, please call us
immediately so that we can arrange to retrieve the original document.
Mabbett & Associates Ltd, Environmental Consultants & Engineers
Lord Hope Building
141 St. James Road
Glasgow, UK
G4 OLT
Tel: 0141 553 2664
Fax: 0141 553 2665
www.mabbett.com
-----Original Message-----
From: Lee Whiteman [mailto:[log in to unmask]]
Sent: 13 January 2005 21:05
To: [log in to unmask]
Subject: Re: [TN] Must we applied N2 to reflow when using Pb-free solder
paste?
Up to a 18 months ago, it was my belief that N2 was required to perform
Lead Free soldering, the rationale being that soldering in N2 would
improve wetting and reduce the amount of residues. However, in building
hardware in our facility (in our LFS course and other customers), I've
come to the conclusion that it is feasible to manufacture Lead Free
soldered hardware without N2. However, the process window is much
narrower.
We found that component preparation, board and component finishes, and
the thermal profile are the prime variables to performing Lead Free
soldering without N2. GIGO - Garbage In, Garbage Out.
We are beginning to perform Lead Free wave soldering in air and
nitrogen. Previous experience with Lead Free wave soldering shows that
N2 will reduce the amount of dross, improve wetting, and reduce the
amount of residures. However, with the new fluxes and alloys available,
N2 may not be required. Stay tuned.
For details and comments, contact me off line.
Lee Whiteman
Senior Manufacturing Engineer
American Competitiveness Institute
E-Mail: [log in to unmask]
Ph: (610) 362-1200 x208
Fax: (610) 362-1290
This message is for informational purposes only and does not supersede,
modify, or create any agreements with ACI. Information contained in this
message does not bind ACI or its affiliates to any commitment, either
express or implied, unless ratified in writing by an authorized
representative.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Krmpotich, Mark
Sent: Thursday, January 13, 2005 3:13 PM
To: [log in to unmask]
Subject: Re: [TN] Antw: [TN] Must we applied N2 to reflow when using
Pb-fr ee solder paste?
Actually it is not all that unique.
We have completed our material and process qualification for lead-free
reflow soldering and have developed a lead-free reflow soldering process
that does not include Nitrogen. It will be going into Hi-Volume
production in April 2005.
Best Regards,
Mark Krmpotich
DFx Engineer
World Wide Operations Technology
Scientific Atlanta
*[log in to unmask]
http://www.scientificatlanta.com/
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ingemar Hernefjord
(KC/EMW)
Sent: Thursday, January 13, 2005 4:17 AM
To: [log in to unmask]
Subject: Re: [TN] Antw: [TN] Must we applied N2 to reflow when using
Pb-fr ee solder paste?
the Swiss are unique....
Ingemar
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Le Ai Quoc
Sent: den 13 januari 2005 09:59
To: [log in to unmask]
Subject: Re: [TN] Antw: [TN] Must we applied N2 to reflow when using
Pb-free solder paste?
Hi Guenter,
Thanks so much for your advice. Actually, your idea is unique on this
net about this topic. It seems nobody use no N2 for reflow. Best
regards, England
----- Original Message -----
From: "Guenter Grossmann" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, January 13, 2005 3:27 PM
Subject: [TN] Antw: [TN] Must we applied N2 to reflow when using Pb-free
solder paste?
> John
>
> Reflow soldering Pb free is possible without N2. You will see some
> problems with wetting. However, the reaction of the solder with the
> metallisation takes place. I heard of rumors about reliability
> problems when soldering without N2 but didn't read a paper so far.
>
> Best regards
>
> Guenter
>
>
>
> EMPA
> Swiss Federal Laboratories for Materials Testing and Research Centre
> for Reliability Guenter Grossmann, Senior Engineer
>
> 8600 Duebendorf
> Switzerland
>
> Phone: xx41 1 823 4279
> Fax : xx41 1 823 4054
> mail: [log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
- - - - - - - Appended by Scientific-Atlanta, Inc. - - - - - - -
This e-mail and any attachments may contain information which is
confidential, proprietary, privileged or otherwise protected by law. The
information is solely intended for the named addressee (or a person
responsible for delivering it to the addressee). If you are not the
intended recipient of this message, you are not authorized to read,
print, retain, copy or disseminate this message or any part of it. If
you have received this e-mail in error, please notify the sender
immediately by return e-mail and delete it from your computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|