hi,
the customer may be concerned that a single ply of prepreg may not provide enough b-stage resin to fill voids in the etched copper foil that you are going to be bonding together. you might want to assure your customer that a single ply will do the trick.
phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ryan Grant
Sent: Thursday, January 13, 2005 4:32 PM
To: [log in to unmask]
Subject: Re: [TN] Butter coat
Whew! Thanks guys, now I don't feel so bad. I thought maybe it was
common knowledge and I'm an idiot for not knowing! The term came from a
customer that demanded our PCB's make use of a "butter coat" if we use
single ply instead of 2 ply prepreg.
-----Original Message-----
From: Brummer Chuck [mailto:[log in to unmask]]
Sent: Thursday, January 13, 2005 11:32 AM
To: 'TechNet E-Mail Forum'; rgrant
Subject: RE: [TN] Butter coat
Ryan,
Did you dig up an old magazine or something? Butter coat is an old and
probably poor term and how much resin is above the glass depends on the
glass style. Prepreg coaters typically squeeze excess resin off the
glass as it is pulled through a trough of resin and then past a bar that
pumps resin through the glass. The meter bars that strip the resin are
set to leave a controlled percentage of resin in and on the glass.
Chuck Brummer
Siemens
-----Original Message-----
From: Ryan Grant [mailto:[log in to unmask]]
Sent: Thursday, January 13, 2005 8:52 AM
To: [log in to unmask]
Subject: [TN] Butter coat
Hi Technetters,
I just learned a new PCB fabrication term today..."butter coat". It's
supposed to be thin layer of resin between glass cloth bundles and
conductors to assure reliability. In the few shop audits I've been
through, I've never seen or heard of a "butter coat". What would the
process look like? Is the resin pressed and frozen into a sheet that
can be handled or would it be squeegy'd on? If it is squeegy'd, can
that be performed by hand or must a machine do it? If a machine must do
it, how do you lay up the brick for the press? Finally, is this a
standard process that I've just been unaware of?
Thanks,
Ryan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|