hi,
if by a visible interface you are talking about different microstructures between the innerlayer foil and the plating in the hole, you are okay. if you are talking about a black interface between the inner layer foil and the plating in the hole, you've got a problem.
phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Finks, Tim
(Healdsburg)
Sent: Monday, January 10, 2005 2:15 PM
To: [log in to unmask]
Subject: [TN] Inner layer to barrel connection quality
I have PTH cross-section images which show a visible interface between inner
layer foils and the PTH plating. Earlier, similar, board cross-sections show
no discernable interface - the inner layer foil and the barrel plating
appear to be integral.
What should I see when I have an acceptable PWB?
Regards,
Tim Finks
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|