Alvin
Solderability testing standard IEC 60068-2-69 (Globule testing for
components) and IEC 60068-2-54 (Solder Bath for boards) are due to be
published this year but I can't give you a date yet. The alloy preferred is
SAC305 although SAC307 and others can also be used. Test temperature is
245DegC.
IPC J-STD002 and 003 is in review. We are just completing a Round-Robin test
programme the preliminary results of which are planned to be reviewed at the
Anaheim meeting Monday 21st Feb....all day!
New spec is planned by year end - if possible. Watch this space.
--
Regards Graham Naisbitt
[log in to unmask]
Wishing you a Happy, Healthy and Prosperous New Year.
Concoat Limited - Engineering Reliability in Electronics
A British Manufacturer
NEW WEB SITE: www.concoat.co.uk :NEW WEB SITE
Cell: 079 6858 2121
Office: +44 (0)1252 813706
On 7/1/05 2:47 am, "Alvin Lua" <[log in to unmask]> wrote:
> thanks werner n daan...i am currently reading up on the info given by both
> of u..wat i need to know now is that, are there any standard tests for the
> solderability of Pb free solders now? any standards for the ageing tests?
> any recommendations of tests n conditions for PbSn n PB free solders? many
> thanks!
>
> regards,
> alvin
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|