I saw a video years ago where the manufacturer was bonding kapton (coverlay
with adhesive) with what looked like a small clothes iron. I don't see why
this same technique would not work for a repair. Since you are bonding to a
relatively flat surface (you don't have to fill copper) it would be worth a
shot. You would need to heat up the coverlay adhesive to the melting point,
apply some pressure and you have a patch. I'm thinking of maybe an LF0220 2
mil Kapton with 2 mils adhesive.
Go to
http://www.dupont.com/fcm/products/H-73245.html for the data sheets.
And, if you try this and it works let us all know.
pete
>From: "Kane, Joseph E (US SSA)" <[log in to unmask]>
>Reply-To: TechNet E-Mail Forum <[log in to unmask]>, "Kane,
>Joseph E (US SSA)" <[log in to unmask]>
>To: [log in to unmask]
>Subject: [TN] Tears In Polyimide/Kapton Flex
>Date: Fri, 7 Jan 2005 13:46:08 -0500
>
>Anyone have a recommendation about an epoxy or other adhesive to
>bond small tears in flex? Of course, these would be tears that don't
>extend into conductors. The material should allow some bend when
>cured.
>
>Joe Kane
>BAE SYSTEMS Controls
>Johnson City, NY
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|