It sounds like you might be describing IPC-7711, Procedure 5.5.4 Gull Wing
installation Hot Air Pencil/Solder Paste Method.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Mary Jane Chism
Sent: Friday, January 07, 2005 12:36 PM
To: [log in to unmask]
Subject: [TN] Soldering 25 mil IC
I have a question for the group on the process of soldering a 25 mil IC.
We have an operator who can remove and replace this IC with a hot air
pencil. She also uses the iron to finishes up the rework by using the
solder iron on any lead that shows an insufficient solder fillet. In
your opinion, is this an "acceptable" process of reworking this
component.
Thanks,
Mary Jane
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|