Hi Roger,
First, you indicate that the PWB design has passed short-term vibration
testing without incident in the past. What exactly is that short-term
vibration testing that the PWB passed? Has a qualification vibration
test or an ESS vibration testing been done? If the answers to the above
questions indicate that the design approach is structurally sound, then
it tends to indicate that the problem is associated with workmanship.
Secondly, does this CCA use ENIG as a final finish on the solder pads?
And if so, have you considered that the presence of ENIG might be
resulting in the "black-pad" contamination issue that is well known as
the Black-line nickel (BLN) low level defect associated with ENIG that
can occur unpredictably for even the best PWB manufacturers, that goes
undetected and ultimately results in improperly formed solder joints
creating failures due to fractures in the solder joints that cause
electrical opens and/or intermittences during ESS vibration and
temperature testing and/or actual field exposures to the same types of
environments.
Regards,
faz
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Roger Stoops
Sent: Thursday, January 06, 2005 1:19 PM
To: [log in to unmask]
Subject: [TN] Solder Joint Failures after Short-term Vibration
Hello all,
We are having an ongoing problem with solder joint failures on a 144-pin
PQFP processor, after short-term vibration. The board layout and
mechanical mounting apparatus were designed with vibration in mind, and
have passed vibration testing in the past. The same processor is used on
a dozen other assemblies, none of which have this problem.
The solder joints appear to exhibit dewetting, although there is a toe
and heel fillet. The heel fillet is unusually large, and the top of the
PQFP lead has a grainy appearance instead of a matte or shiny
appearance. Some leads can be pushed off the solder joint with very
little pressure. Sn62Pb36Ag2 solder is being used, and our EMS provider
continues to claim that boards meet IPC-A-610 class 2 requirements.
Any ideas as to what may be causing solder joint failures?
Also, any suggestions or recommendations (preferred) for a test house to
provide x-ray, microsection and composition analysis?
TIA & Best Regards,
Roger M. Stoops, CID+
Trimble Navigation Ltd., Dayton, OH, USA
Ph: +01 937.245.5288
Fax: +01 937.233.7511
Oh, and BTW, changing EMS providers is not an option...
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
******************************************
The information contained in, or attached to, this e-mail, may contain confidential information and is intended solely for the use of the individual or entity to whom they are addressed and may be subject to legal privilege. If you have received this e-mail in error you should notify the sender immediately by reply e-mail, delete the message from your system and notify your system manager. Please do not copy it for any purpose, or disclose its contents to any other person. The views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of the company. The recipient should check this e-mail and any attachments for the presence of viruses. The company accepts no liability for any damage caused, directly or indirectly, by any virus transmitted in this email.
******************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|