TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Pete menuez <[log in to unmask]>
Date:
Thu, 27 Jan 2005 10:17:49 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Vladimir Igoshev <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Vladimir Igoshev <[log in to unmask]>
Parts/Attachments:
text/plain (83 lines)
Hi Pete,

Here are some answers;

1. The cross head speed of a tensile machine is set in "unit of length"/"unit of time" (mm/sec, for instance). The IPC spec you referred to says "per minute of the length of the reduced section", which basically means the gage length. In other words, the spec talks about the deformation, not elongation rate. It's a common approach in materials testing.
In general, the cross head speed could affect the deformation (again, not elongation) value but it shouldn't be the case for your test.

2. In general it's not true. But again, one should talk about deformation not elongation. Elongation will always increases with increasing in the gage/sample length. However, the tensile strength, for the same material won't change simply because it depends on the material properties, but not the sample size.

3. The presence of humidity in a sample (board) could change it's mechanical properties.

Hopefully, it will help.

Regards,

Vladimir



Vladimir Igoshev, Ph. D.
Senior Materials Researcher
Research in Motion
451 Phillip St.
Waterloo, ON, N2L 3X2

Voice: (+1) 519-888-7465, ext. 5283
Fax: (+1) 519-886-0863
E-mail: [log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Pete menuez
Sent: Thursday, January 27, 2005 8:37 AM
To: [log in to unmask]
Subject: [TN] Tensile Strength and Elongation Questions


Group:

I have a some questions regarding T/E I'm hoping someone can help.

1. IPC-TM-650  2.4.18.1A  paragraph 5.3.4.2 requires a Cross head speed of
between .05 - .5mm/mm (.00197-.0197 in/in) but does not specify the speed to
use in the test. It seems to me that the cross head speed could affect the
elongation values.  The slower the speed the higher the elongation.  Is
there any validity to my thought or does speed not make a difference?

2. Tensile strength and elongation have an inverse relationship.  Higher
elongation = lower tensile.  Is this true?

3. Paragraph 5.2 requires a Pre Test bake.  Why? Does this bake affect T/E?
What if the board shop also baked the sample for 4 - 6 hours - Would a
double bake have twice the affect.

Thanks in advance for any help.

pete

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2