Cheryl's point on 2ndary reflow is a good one. I"ve seen this a couple of
times. Also, the fix of changing the wave solder parameters is good too.
Another idea for corrective action, if changing the wave parameters is not
a good choice is to add a thermal barrier to the area under the QFP on the
bottom side of the PCB. Polyimide tape (Kapton) works good for this. A
longer term fix may also be to mask over the vias in that area under the
QFP. The mask can provide enough of a thermal barrier to prevent 2ndary
reflow.
Kelly
On Thu, 6 Jan 2005 12:27:31 -0600, Cheryl Tulkoff <[log in to unmask]>
wrote:
>Roger -
>
>Does this board go through the wave solder process after SMT? You could be
>seeing secondary reflow of the SMT joint at the wave. This happens when the
>temperature of the wave process is sufficient to remelt topside joints. It
>usually happens only on fine pitch QFPs(smaller joints with less solder
>volume). To avoid this, most people will run the wave solder temperature
>lower (240-250 C rather than 260C) and the conveyor faster (5.5 ft/min or
>higher).
>
>I can send more info if you're interested in checking it out.
>
>Thanks,
>
>Cheryl Tulkoff
>Phone:(512) 683-8586
>Fax: (512) 683-8847
>National Instruments
>11500 N. Mopac Expressway
>Building A
>Austin, TX 78759-3504
>
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|