TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 21 Jan 2005 07:55:36 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Richard Kraszewski <[log in to unmask]>
Parts/Attachments:
text/plain (109 lines)
Nope. QQS-571E is not appropriate here either. QQS571E does contain
recommended impurity levels for at least one Pb-free alloy (Sn96) but if
my memory serves me correctly, it is primarily a purchasing spec for
tin/lead alloys. 

In light of there even being so much debate & discussion concerning the
long performance of SAC alloys as compared to 63/37, I can't see how any
industry body is willing to write a spec covering the manufacturing
induced impurities and their acceptable levels.  Some impurities may be
rather obvious (ie., S, P As, Al,) but determining the acceptable level
of say Cu over the whole range of SAC alloys will be considerably more
challenging.

I suspect these impurity limit levels will not be reliably set until
some years after the industry transitions to more of a lead-free
manufacturing base.

Rich K / KEDS
 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Edwin Louis
Sent: Friday, January 21, 2005 7:37 AM
To: [log in to unmask]
Subject: Re: [TN] Lead-free Wave Solder Pot Impurity Levels


What about Federal Specification QQS-571?

-----Original Message-----
From: Leland Woodall [mailto:[log in to unmask]]
Sent: Friday, January 21, 2005 6:26 AM
To: [log in to unmask]
Subject: [TN] Lead-free Wave Solder Pot Impurity Levels


Hi Folks,

I have a small dilemma here.  There is a standard for eutectic solder
pot impurity levels, but I can't seem to find one for lead-free.  Is
there such an animal?

Everything I've researched on the Web shows only recommendations, namely
from Alpha and AIM.  Those two have slight disagreements.
At least they provide something, and that is impressive.

It also appears that the major concern is processing problems versus
product reliability.  If copper content gets too high, the wave solder
viscosity becomes too high and bogs down the mechanical parts of the
machine.

When things get out of whack, can I expect reliability problems as well?

What levels of impurities would cause premature joint failure,
specifically?

Are we too new to this, and have tests not yet been agreed upon?  Is IPC
addressing the issue?

Any help you could provide would be sincerely appreciated.

Offline comments are welcomed.

Many, many thanks,

Leland Woodall
Quality Coordinator

Keihin Carolina System Technology, Inc.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2