B-488 Type = gold purity.
Type I = 99.7%
TypeII = 99.00%
TypeIII = 99.9%
B488 is an electroplated gold spec.
I don't have a copy of the nickel spec, sorry. All are available on line at
www.sae.org
pete
>From: John Parsons <[log in to unmask]>
>Reply-To: TechNet E-Mail Forum <[log in to unmask]>, John Parsons
><[log in to unmask]>
>To: [log in to unmask]
>Subject: [TN] ASTM Specification Reference Required
>Date: Thu, 20 Jan 2005 08:50:49 -0800
>
>Good morning all,
>
>We are quoting on a job (PCB Fab) and the specifications reference the
>following ASTM Specifications;
>- B689-97, (Nickel Plating) Type 1 or Type 2 plate, min thickness 3 micron
>-B488-01, (Gold Plating) Type I or III gold, min thickness 0.3micron.
>
>I do not have ready access to copies of the ASTM specs. Can anyone cross
>these to equivalent IPC spec's or at the least, interpret these for me into
>PCB speak :) .
>
>Regards
>John Parsons
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|