TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Pete menuez <[log in to unmask]>
Date:
Thu, 6 Jan 2005 04:35:55 +0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Muthu <[log in to unmask]>
Subject:
From:
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (188 lines)
We want to reduce the cycle time for laying 5mil together with 1 mil
STF..Hence we are looking for solid 6mil stf..

M Muthu
Product Engineering Dept
No. 99 Lebuhraya Kampung Jawa
Taman Perindustrian  11900 bayan Lepas
Penang, Malaysia

Tel : 6420000
Fax: 6482222

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Pete menuez
Sent: Tuesday, January 04, 2005 5:15 AM
To: [log in to unmask]
Subject: Re: [TN] 6 Mils STF

You could use a piece of Dupont LF0150 or LF0250.  This is 5 mils +
adhesive.  The problem with this is drilling the kapton.  It tends to tear
or shred and when you press it on you can get little stringers which may
affect the annular ring.

Another solution might be to take a piece of 3 or 4 core polyimide (or FR4)
with some prepreg (106 no flow?) and bond this on the board.  The stiffner
and prepreg should drill fairly well.

Good luck.

pete


>From: Brummer Chuck <[log in to unmask]>
>Reply-To: TechNet E-Mail Forum <[log in to unmask]>,              Brummer
>Chuck <[log in to unmask]>
>To: [log in to unmask]
>Subject: Re: [TN] 6 Mils STF
>Date: Mon, 3 Jan 2005 08:31:10 -0800
>
>But DuPont does not provide Kapton in this thickness.
>
>Fralock has a license in which they bond two layers or either 2 mil or 3
>mil
>Kapton and call it Cirlex.  We have been trying to work this into some
>applications and are not yet successful.
>
>Chuck Brummer
>Siemens
>
>-----Original Message-----
>From: Marvin Gaines [mailto:[log in to unmask]]
>Sent: Tuesday, December 28, 2004 12:52 PM
>To: [log in to unmask]
>Subject: Re: [TN] 6 Mils STF
>
>
>Kapton should work.
>
>DuPont sells this material
>
>Ted Gaines
>Multi Fine line Electronix
>www.mflex.com
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Muthu
>Sent: Sunday, December 26, 2004 12:53 PM
>To: [log in to unmask]
>Subject: Re: [TN] 6 Mils STF
>
>Hi,
>
>We are looking for 6 mils Polymide Stiffener to strengthen the finger areas
>on flexible PCB.
>
>Can anybody advice about the vendors supplying above Stiffener.
>
>Thanks in advance.
>M Muthu
>Product Engineering Dept
>No. 99 Lebuhraya Kampung Jawa
>Taman Perindustrian  11900 bayan Lepas
>Penang, Malaysia
>
>Tel : 6420000
>Fax: 6482222
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of [log in to unmask]
>Sent: Saturday, December 25, 2004 1:16 AM
>To: [log in to unmask]
>Subject: Re: [TN] Purple pads / corrosive ? pads
>
>Dave is correct re storage. Had a customer that complained about 'residue'
>which turned out to be silver sulfide. On-site inspection showed PWBs and
>parts
>were stored adjacent to the cafeteria serving line-- which featured
>scrambled
>eggs every morning. Once the parts were re-located, the residue
>disappeared--
>leaving the customer with egg on face but no residue on parts.
>
>Bill Kenyon
>Global Centre Consulting
>3336 Birmingham Drive
>Fort Collins, CO   80526
>Tel: 970.207.9586   New Cell: 970.980.6373
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2