To paraphrase Winston Churchill... Many forms of 'surface finish' have been
tried, and will be tried in this world of sin and woe. No one pretends that
'OSP' is perfect or all-wise. Indeed, it has been said that 'OSP' is the
worst form of 'surface finish' except all the others that have been tried
from time to time.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Cheryl Tulkoff
Sent: Friday, January 14, 2005 11:55 AM
To: [log in to unmask]
Subject: Re: [TN] OSP Board Finish
We've reduced OSP for a few reasons:
1. Reduced cost and increased availability of other finishes - like
immersion silver
2. Ability to ICT test without solder on the test pads (avoids no clean
residue contact problems)
3. Ability to set up good, flat grounding areas on the PCB
Thanks,
Cheryl Tulkoff
Phone:(512) 683-8586
Fax: (512) 683-8847
National Instruments
11500 N. Mopac Expressway
Building A
Austin, TX 78759-3504
Dennis Manowski
<boardmanusa@YAHO
O.COM> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
01/14/2005 12:56 [TN] OSP Board Finish
PM
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Dennis Manowski
<boardmanusa@YAHO
O.COM>
Does anyone know why the use of SMT PCB's with OSP finish has dropped off
as much as it has ?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|