Bill
You can strip IAg. The cost so the supplier is usually between HASL and
ENIG, but cost is seldom the only price driver.
Best regards
Lee
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brooks,Bill
Sent: Friday, December 03, 2004 2:50 PM
To: [log in to unmask]
Subject: Re: [TN] HAL Finish/IAg/ENIG/OSP...
Yea.. but whose counting?
LOL
It started out to be one question... but as I typed it I had more.. I
should
have gone back to update the count there... but yea... its Friday...
almost
lunch time...
:)
So it sounds like Immersion Silver has the best of all worlds with the
one
caveat in the presence of sulpher it can be nasty... but even then...
can't
the board be stripped and replated to recover it? Is that costly?
I really see no downside to silver immersion then... unless there is
something that hasn't been covered... compatibility with all processes,
not
even ionic contamination issues in the washing process... no issues?...
I like it.
I may have a talk with our MFG ENG and see what he thinks of switching
from
ENIG to IAg. For our fine pitch parts. Getting the nickel out of the
process
is probably a good thing...for RF.
What about cost vs. IAg?
Best regards,
Bill Brooks - KG6VVP
PCB Design Engineer , C.I.D.+, C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
e-mail:[log in to unmask]
http://www.dtwc.com
http://pcbwizards.com
-----Original Message-----
From: Wenger, George M. [mailto:[log in to unmask]]
Sent: Friday, December 03, 2004 11:29 AM
To: TechNet E-Mail Forum; Brooks,Bill
Subject: RE: [TN] HAL Finish
Bill,
It is Friday and I had a rough week. I missed the fact that you
actually
asked 6 questions.
5. Yes but not significantly.
6. Yes it will but if the Pb-Free is SAC you'll not be able to measure
the
small amount of Ag contamination.
Regards,
George
George M. Wenger (908)-546-4531
Reliability / FMA Engineer
Base Station and Subsystems Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Wenger, George M.
Sent: Friday, December 03, 2004 2:09 PM
To: [log in to unmask]
Subject: Re: [TN] HAL Finish
Bill,
You start out saying "One question I would have regarding Immersion
Silver"
and then you ask 4 questions.
here are my answers to the 4 questions.
1.nothing
2. Nothing significant
3. No
4. No
Regards,
George
George M. Wenger (908)-546-4531
Reliability / FMA Engineer
Base Station and Subsystems Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Brooks,Bill
Sent: Friday, December 03, 2004 1:55 PM
To: [log in to unmask]
Subject: Re: [TN] HAL Finish
One question I would have regarding Immersion Silver. What does it do to
the
solder metallurgically? Anything at all? Do they require an under
plating
barrier for immersion silver like they do with the nickel/gold immersion
gold process? Is there a silver dendrite issue?
If you were using a wave solder process with surface mount would the
silver
contaminate the bath over time? What about lead free wave solder?
There are so many things that affect the decision to go with a process
that
are not just joint quality related...
The world keeps turning and the only constant is change itself...
Best regards,
Bill Brooks - KG6VVP
PCB Design Engineer , C.I.D.+, C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
e-mail:[log in to unmask]
http://www.dtwc.com
http://pcbwizards.com
-----Original Message-----
From: Roger Stoops [mailto:[log in to unmask]]
Sent: Friday, December 03, 2004 10:30 AM
To: [log in to unmask]
Subject: Re: [TN] HAL Finish
Their email just said they wanted lead-free HAL, no IAg. Then they said
"...Immersion Silver is not suitable for long storage which is leading
to
other problems." Like Lee said, bizarre! What is long-storage?
Anything
over 6-12 months is not good anyway for lean/JIT manufacturing, or so I
thought.
Got some boards from a reputable fab house with IAg plating just this
week,
and they were packaged to last a long time: sulfur-free paper between
each
board, 10 boards per well-sealed shrink wrap plastic pack with desiccant
inside pack. Sounds like they have their act together, no?
But sometimes we are required to use certain vendors, and I have to make
my
designs compatible with each one...and not necessarily all at the same
time.
BRgds,
Roger
Like Courage says, "What I do for love..."
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Wenger, George M.
Sent: Friday, December 03, 2004 12:12 PM
To: [log in to unmask]
Subject: Re: [TN] HAL Finish
Did your EMS vendor give you any reasons why they will not accept boards
with IAg plating. It tould be good to know if they have documentation
of a
problem or if they simply have a fear.
Regards,
George
George M. Wenger (908)-546-4531
Reliability / FMA Engineer
Base Station and Subsystems Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Roger Stoops
Sent: Friday, December 03, 2004 12:08 PM
To: [log in to unmask]
Subject: [TN] HAL Finish
One of our EMS vendors has told us they will not accept boards with IAg
plating. Instead, they want HAL, which I assume they want hot-air
leveled
Sn.
Any pros and cons anyone would like to share from the board fab,
assembly
and test viewpoints? Any advantage to plating Sn over Ni, or just a
waste
of money/not necessary?
Many thanks in advance,
Roger
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------
----
--------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------
----
--------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------
----
--------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------
----
--------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------
----
--------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------
----
--------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|