Al: Assume the change to Silver has cured the problem?
Immersion Tin can be a bit of a problem to rinse, as it tends to gel when cooled. We advise our customers to have a heated (warm) first rinse, which makes this problem go away.
Rudy Sedlak
RD Chemical Company
---------------------------------